EICP加固饱和砂土的电阻率响应特征与渗透性关联研究

    THE CORRELATION BETWEEN RESISTIVITY RESPONSE CHARACTERISTICS AND PERMEABILITY IN EICP-TREATED SATURATED SAND

    • 摘要: 酶诱导碳酸钙沉淀(EICP)技术是加固饱和砂土、降低其渗透性的有效方法,但实现其加固效果的无损检测是推动其大规模工程应用的关键。本文通过溶液试验、米勒盒试验及砂柱固化试验,研究胶结液浓度、注浆次数、注浆量等关键参数对孔隙水电阻率、饱和砂土电阻率及渗透系数的影响规律,探讨利用电阻率法原位评估EICP加固效果的可行性。结果表明:孔隙水电阻率随胶结液浓度增加呈指数下降,但高浓度下敏感性降低;多轮注浆下,孔隙水离子不断累积导致其电阻率先快速下降,约4~5轮注浆后趋于稳定。饱和砂柱的整体电阻率随注浆呈现先下降后上升的非单调变化,转折点出现在第4~5轮注浆,其物理机制由早期孔隙水离子浓度控制向后期碳酸钙沉淀致孔隙结构变化控制转换。碳酸钙生成量与分布是影响固化土体电学与渗透性能的核心因素,结石体电阻率与渗透系数随胶结液浓度提高呈现下降趋势,两者通过“渗透性-碳酸钙含量-电阻率”紧密关联。空间电阻率检测揭示EICP加固效果沿渗流路径的不均匀性,下部试样因反应更充分而表现出更早的电阻率转折与更强的胶结加固效应。该研究结果验证了电阻率法作为EICP技术加固饱和砂土的无损检测手段的可行性,为EICP技术的发展提供重要检测技术支持。

       

      Abstract: Enzyme Induced Calcium Carbonate Precipitation (EICP) can effectively consolidate saturated sand and reduce its permeability. However, non-destructive monitoring of the reinforcement effect is crucial for large-scale engineering application. This study investigates the influence of cementation solution concentration, grouting frequency, and grouting volume on the resistivity and permeability of EICP-treated saturated sandy soil, and evaluates the feasibility of resistivity-based in situ assessment. Experiments include solution tests, Miller box tests, and sand column consolidation tests. Results show that pore water resistivity decreases exponentially with cementation solution concentration, though sensitivity diminishes at higher concentrations. Under multiple grouting cycles, continuous ion accumulation causes a rapid drop in resistivity, which stabilizes around the 4th~5th cycle. By contrast, the resistivity of the saturated sand column exhibits a non-monotonic trend, first decreasing and then increasing. The turning point at the 4th~5th cycle reflects a shift in the dominant mechanism from pore-water ion concentration control to pore-structure alteration caused by calcium carbonate precipitation. Calcium carbonate formation and distribution govern the electrical and permeability properties of the cemented soil. Both resistivity and permeability decrease systematically with increasing cementation solution concentration, a phenomenon that can be explained by the permeability-CaCO3 content-resistivity relationship. Spatial monitoring further reveals non-uniform reinforcement along the seepage path: lower sections, where reactions are more complete, exhibit earlier resistivity transitions and stronger cementation. This study demonstrates the viability of resistivity-based non-destructive testing for EICP-reinforced saturated sand, providing important technical support for advancing EICP technology.

       

    /

    返回文章
    返回