孔隙玄武岩CO2矿化反应与封存效率实验研究

    EXPERIMENTAL STUDY ON CO2 MINERALIZATION AND STORAGE EFFICIENCY IN POROUS BASALT

    • 摘要: 玄武岩碳封存以矿化封存为主,针对孔隙结构中CO2矿化反应难以准确描述的问题,以海南琼北地区玄武岩为对象,在30 ℃、6 MPa初始反应压力下,开展了38~43 μm、63~75 μm粉末和25 mm×5 mm孔隙结构岩样的30 d矿化反应实验,分析了孔隙结构对反应路径和封存效率的影响。主要发现如下:(1)孔隙结构会显著降低矿化反应速率。二价阳离子浓度整体表现为Ca2+>Fe2+>Mg2+,但在孔隙尺度下该趋势出现最晚;反应至第30 d,孔隙尺度下Ca2+、Fe2+、Mg2+的离子释放速率仅为粉末样品的0.2倍、0.5倍和0.17倍。(2)矿化产物因玄武岩形态不同而存在差异。粉末样品反应后可生成CaCO3,TGA热重当量约为10.19 wt%,与XRD测试结果(9.13 wt%)基本一致;孔隙结构样品碳酸盐热信号较弱,TGA与SEM-EDS表明矿化产物以黏土/铝硅酸盐类次生相为主,碳酸盐矿化程度有限。(3)封存效率差异显著。孔隙结构样品CO2表观消耗效率为0.842%,低于38~43 μm和63~75 μm粉末样品的5.08%和4.91%;CO2表观消耗量为27.09 kg ·t-1,仅为粉末样品的13% ~14%。TGA证实粉末样品固相碳酸盐固定CO2量约44.80 kg ·t-1,孔隙结构样品仅约4.25 kg ·t-1,说明低pH下孔隙结构玄武岩碳酸盐矿化程度受限。研究表明粉末样品矿化结果不能直接外推至真实地质储层,工程设计应以孔隙结构的结果为主要依据,动态优化封存工艺,以提升CO2矿化反应速率及封存量。

       

      Abstract: Basalt carbon storage holds promise for fundamentally addressing engineering challenges such as CO2's tendency to leak and the difficulty of long-term storage. The CO2 mineralization reaction mechanism within pore structures is the core of basalt carbon storage. To tackle the problem of accurately describing CO2 mineralization reactions within pore structures, this study took basalts from the northern Qiong area of the Leizhou Peninsula as the research subject. Under unified reaction conditions (30 ℃, 6 MPa CO2-saturated solution, 30 days), experiments on CO2 mineralization reaction and storage efficiency were conducted using basalt samples of different scales. The study analyzed the dissolution intensity and rates of different divalent cations, the distribution and impact of secondary minerals within pores of different scales, as well as CO2 mineralization efficiency and storage capacity. The main findings are as follows: (1) The pore structure of basalt reservoirs significantly retards and inhibits the CO2 mineralization reaction. Although the overall cation dissolution concentration followed the order Ca2+>Fe2+>Mg2+, this trend emerged latest at the pore scale, with the concentrations of the three ions being only 0.29, 0.39, and 0.47 times those in 38~43 μm powder samples, respectively. By day 30 of the reaction, the ion release rates at the pore scale were only 0.2 times(Ca2+), 0.5 times(Fe2+), and 0.17 times(Mg2+) those of the powder samples. (2)Mineralization products varied with basalt sample morphology. Powder samples produced CaCO3 after reaction, with a TGA-derived carbonate equivalent of approximately 10.19 wt%, in good agreement with the XRD-determined value of 9.13 wt%. In contrast, the porous core samples exhibited markedly weaker carbonate thermal decomposition signals; combined TGA and SEM-EDS analysis indicated that the mineralization products were dominated by clay minerals and aluminosilicate secondary phases, with carbonate mineralization remaining limited. (3) Significant differences in CO2 sequestration efficiency were observed between sample types. The apparent CO2 consumption efficiency of the porous core samples was only 0.842%, substantially lower than the 5.08% and 4.91% recorded for the 38~43 μm and 63~75 μm powder samples, respectively. The corresponding apparent CO2 consumption was 27.09 kg- · t-1, representing merely 13% ~14% of that achieved by the powder samples. TGA further confirmed that the solid-phase carbonate-bound CO2 in powder samples reached approximately 44.80 kg- · t-1, whereas that in porous core samples was only about 4.25 kg- · t-1. These results demonstrate that, under low-pH conditions, carbonate mineralization in intact porous basalt is considerably constrained, likely owing to the limited reactive surface area accessible within the pore network. This research reveals that pore structure is a key factor constraining the rate, efficiency, and capacity of CO2 mineralization reactions. In the prediction and assessment of storage projects, the influence of pore structure should be dynamically considered, and storage processes should be optimized in real time to enhance the CO2 mineralization reaction rate and storage capacity.

       

    /

    返回文章
    返回