    酸雨淋溶下MICP固化铅污染土的淋滤特性研究

    LEACHING CHARACTERISTICS OF MICP SOLIDIFIED LEAD-CONTAMINATED SOIL UNDER ACID RAIN LEACHING CONDITIONS

    • 摘要: 酸雨可与MICP矿化作用过程中生成的碳酸盐反应,破坏材料的结构强度,使被固定的重金属离子再次释放,但该技术在酸雨环境下的研究较少,耐酸腐蚀性尚不明确,因此对酸雨入渗作用下MICP固化重金属污染土的淋滤特性的研究具有现实意义。本文设计了pH值为3.5、4.5、5.6的3种典型的酸雨条件,用pH值为7.5的去离子水作对照,通过土柱淋滤的方法对MICP固化粉土进行了实验研究,分析不同酸雨pH值对MICP固化铅污染土样的强度、pH值、Pb2+、Ca2+淋出量及Pb2+赋存形态的影响。结果表明:随酸液pH值降低,MICP固化试样的强度降低,淋出液pH值降低,Pb2+、Ca2+淋出量增加,固化试样中可交换态的Pb2+增加,当pH值为5.6时,试样受酸雨影响较小,pH值降为3.5时,试样变化显著。

       

      Abstract: Acid rain can react with carbonate formed in the process of MICP mineralization,destroy the structural strength of materials and release the fixed heavy metal ions again.However,the research on this technology in acid rain condition is less,and the acid corrosion resistance is not clear.Therefore,it is of practical significance to study the leaching characteristics of MICP solidified heavy metal contaminated soil under acid rain infiltration.In this paper,three typical acid rain conditions with a pH of 3.5,4.5 and 5.6 were designed.Deionized water with a pH of 7.5 was used as a control.The experimental study on MICP solidified lead-contaminated soil was carried out by using soil column leaching method.The influence of pH value of acid rain on strength,pH value,leaching amount of Pb2+,Ca2+ and occurrence form of Pb2+ was analyzed.The results show that: as the pH value of acid solution decreases,the strength of MICP solidified sample decreases,But as the pH value of leaching solution decreases,the leaching amount of Pb2+ and Ca2+ increases,When the exchangeable Pb2+ in solidified sample increases,and the Pb2+ in carbonate bound,iron manganese oxide bound,organic matter bound and residue state would decrease.The sample would be less affected by acid rain of 5.6 pH,while the pH value is 3.5,the sample change significantly.

       

    /